检查井通病原因分析
Analysis of causes of common faults in inspection wells
1.1施工工艺所致
1.1 the result of construction process
施工工艺是检查井质量控制消除病害的关键环节,施工质量的优劣直接影响着检查井的使用效果。其原因主要存在以下三个方面
The construction technology is the key link to control the quality of the inspection well and eliminate
www.kelinbaojie.cn www.dzhlzj.com www.aohailaowu.com www.fanguangmo51.com www.beijingqima.cn www.tianchengwuzi.com.cn4000312797the disease. The quality of the construction directly affects the use effect of the inspection well. The main reasons are the following three aspects
(1) 检查井地基承载力不够。路面上的重力动荷载是通过检查井的井盖传至检查井井体,再通过井体垂直作用于地基上,即路面检查井上的车荷载最终是作用在检查井地基上的。这就要求检查井地基的承载力必须达到一定的强度,否则在上部长时间动荷载的作用下 ,地基土就会被压缩下沉,致使检查井整体下沉 ,检查井出现凹陷,路面不平整
(1) the bearing capacity of the inspection well foundation is not enough. The gravity dynamic load on the pavement is passed through the cover of the well to check the well body, then the vertical action of the well body on the foundation, that is, the vehicle load on the pavement inspection well is ultimately on the inspection of the well foundation. This requires that the bearing capacity of the foundation of the inspection well must reach a certain strength, otherwise the foundation soil will be compressed and sink under the action of the long time moving load on the upper part, resulting in the overall sinking of the inspection well, the inspection well and the unevenness of the pavement.
(2) 压实度不达标。路面结构与检查井的刚度相差大,存在刚性与柔性转换问题。保证井周回填土压实度至关重要。根据《给水排水工程构筑物施工及验收规范》(G B5014 1—2008) ,检查井周围回填土的压实度应当与道路基层压实度相同,即压实度应大于等于 95 %(重型压实标准 ),但在井施工过程中普遍做法是在井筒砌筑完成后,井与工作坑之间距离狭小,导致机械碾压困难 ,一般绕
(2) the degree of compaction is not up to standard. There is a big difference between the stiffness of the pavement structure and the inspection shaft, and there is a problem of rigidity and flexibility conversion. It is very important to ensure the compaction degree of the backfill soil. According to the code for construction and acceptance of water supply and drainage engineering structures (G B5014 1 - 2008), the compaction degree of backfill surrounding the well should be the same as that of the road base, that is, the compaction degree should be equal to 95% (heavy compaction standard), but the common practice in the well construction process is the well and the working pit after the wellbore is built. The distance between them is narrow, resulting in difficulty in mechanical rolling and general winding.
过井一定距离碾压;而人工夯实又难 以控制质量,从而导致井周回填土在使用过程中逐渐沉降,引起井周路面下沉,检查井四周开裂。
It is difficult to control the ramming of the cross well, and it is difficult to control the quality by artificial tamping, which leads to the gradual settlement of the backfill soil during the use of the well, causing the sinking of the circumferential pavement and checking the cracks around the well.
(3) 施工时高程控制不严格及施工工期的压缩。很多施工单位都是在道路侧石砌筑完成后,参照侧石的标高确定井盖的标高。忽略了道路的横向坡度,使井盖标高和道路设计标高不协调,检查井盖高出或低于路面,在使用过程中受到车辆荷载冲击作用后会加剧井盖与井周路面的不均匀沉降
(3) the height control is not strict during construction and the construction period is compressed. Many construction units determine the elevation of the well cover according to the elevation of the side stone after the completion of the side stone masonry. The lateral slope of the road is ignored, which makes the height of the shaft cap uncoordinated with the road design elevation, and the cover of the well is higher or lower than the road surface. The uneven settlement of the shaft cover and the well surface will be aggravated by the impact of the vehicle load during the use process.
(4) 市政道路行业的施工工期压缩也是造成检查井病害的一
(4) construction period compression of municipal road industry is also one of the diseases causing inspection wells.
个不容忽视的原因。混凝土达到设计强度所需时间都在 28d 以上,若工期安排不合理,在混凝土强度还未形成前就进行碾压,极易造成施工期间的破坏;另一方面养护时间达不到要求,施工单位为避免重夯造成井身变形 ,不敢对井周回填土进行较强夯实。
A reason that can not be ignored. The time required for the concrete to achieve the design strength is more than 28d. If the schedule is not reasonable and the concrete strength has not been formed before the concrete strength is formed, it is very easy to cause damage during the construction period; on the other hand, the maintenance time can not reach the requirement. The construction unit can avoid the shape of the well body to avoid the heavy ramming, and dare not to carry on the comparison of the backfill soil in the well. Strong tamping.
1.2检查井支座松动,井周路面沥青面层开裂。新晋祠路开井后发现,多数该类检查井井筒完好,井盖和支座均出现了松动,支座下的座浆和井内抹面出现不同程度的脱落。
1.2 the bearing of the inspection well is loose, and the asphalt pavement surface cracks on the well side. After the opening of the new Jinci Road, it is found that most of this kind of inspection well bore is intact, the cover and support of the well have been loosened, and the slurry and the hole surface under the support have different degrees of falling off.
上一页  检查井钢模具的生产及维护  
下一页  混凝土检查井施工要求
  • 关于我们
  • 新闻动态
  • 案例展示
  • 网上订单
  • 联系我们
  • 产品分类1
  • 产品分类2
  • 产品分类3

Copyright © 技术支持:遨游网络

  • 联系我们
  • 网上订单
  • 工程案例
  • 本站导航

搜索

  • 关于我们
  • 新闻动态
  • 案例展示
  • 网上订单
  • 联系我们
  • 产品分类1
  • 产品分类2
  • 产品分类3